Waviness and Ra control on mechanical seal faces
XZ-230 revealed Ra of 0.08 µm passing while waviness of 0.4 µm failed; after l…
Field results by industry, with cycle time, yield and cost impact

XZ-230 revealed Ra of 0.08 µm passing while waviness of 0.4 µm failed; after l…

Y9025C measured three sections and ran a waviness spectrum, identifying sixth-…

CX-3/100 showed Ra within spec but Rmr only 42%, indicating an insufficient pl…

CX-3/160 profilometry to ISO 4287 revealed that early port-plate wear traced t…

The CX-3/160 measures Ra and crown in one setup, cutting inspection from 35 to…

Y9025C with 0.02 um spindle accuracy replaced sparse CMM sampling, exposing 0.…

MARSURF-XCR20 evaluates Rk, Rpk and Rvk of plateau honing per ISO 13565-2; tig…

MARSURF-XC2 with a small-bore stylus reaches module-2 tooth spaces, grading Ra…

XZ-150G measures seal-land contour, chamfer angle and fillet radius of 15000 r…

XZ-400 scans gothic-arc raceways over 400 mm travel at 0.02 um resolution, rep…

Y9025B with 0.025 um spindle accuracy verifies spool roundness at 0.3 um and c…

MARSURF-UD130 with 0.3 nm vertical resolution spot-checks polished SiC substra…

MARSURF-LD260 replaces interference-band reading with 0.1 um straightness metr…