Polished 6-inch SiC substrates require Ra ≤0.2 nm. All checks were outsourced to AFM with a 4-hour turnaround per batch, so slurry recipe corrections lagged badly and outgoing Ra drifted between 0.10 and 0.18 nm.
Solution: a MARSURF-UD130 ultra-precision profilometer with 0.3 nm vertical resolution and a 0.05 mN measuring force to avoid scratching, grading Ra and Rq per ISO 4287. Five points per wafer (centre and edge), scanned at 0.1 mm/s to suppress vibration noise.
Results: same-wafer correlation with AFM reached 0.95 with deviation ≤0.02 nm. Batch turnaround fell to 25 minutes, slurry corrections moved three hours earlier, outgoing Ra stabilized at 0.12 nm, and epitaxy customer complaints dropped to zero.