Motor shafts for 15000 rpm e-drives rely on seal-land contour and chamfer angle to set lip contact pressure. Profile projectors with ±5 um reading error were used for spot checks, and early leakage ran at 0.8%.
Solution: an XZ-150G high-precision profilometer measures seal-land contour, chamfer angle, fillet radius and bearing-seat straightness in one clamping, using a 2 um stylus tip with 0.02 um Z resolution; measured profiles are least-squares fitted against the nominal CAD contour.
Results: seal-land contour was tightened from 3 um to 1.5 um and the 25°±0.5° chamfer fully controlled. Early leakage fell to 0.1%, saving about 2 million yuan a year in warranty claims, with a 2-minute cycle enabling 100% inspection.