PCB micro-sectioning for hole-wall copper and resin voids
Precision sectioning plus vacuum mounting delivers results in 35 minutes with …
Field results by industry, with cycle time, yield and cost impact

Precision sectioning plus vacuum mounting delivers results in 35 minutes with …

Low-speed sectioning with vacuum mounting and electrolytic polishing cut coati…

HXZDQ-160 mounting with HXZMP-3000 automatic polishing completes six samples i…

An HXZDQ-160 + HXQ-100 + HXZMP-2000 line raised PQR section acceptance from 85…

Q-2 saw, XQ-2B press and MP-2 dual platen raised output from 40 to 85 samples …

HXZDQ-100Z low-speed precision cutting prevents burn on SLM TC4 coupons; with …

HXZMP-3000 prepares six WC-Co inserts per load per ISO 4499, with 100% repeata…

HXSQ-100F low-speed sectioning avoids chipping on TiAlN-coated inserts; optica…

HXZDQ-120 wet metallographic cutting with low feed keeps the burn layer within…

HXZMP-2000Z automatic preparation of GCr15 bearing rings avoids inclusion pull…

HXZMP-1000 with 10% oxalic electrolytic etch prepares 304 stainless weld sampl…

HXZMP-1000Z automatic prep with caustic etch reveals flow-line continuity and …

HXQ-50 hot mounting at 180°C/25 MPa prepares connector crimp cross-sections; p…