Semiconductor2025

MARSURF-UD130 for Nanometre Roughness of SiC Substrates

MARSURF-UD130 with 0.3 nm vertical resolution spot-checks polished SiC substrates, correlating with AFM at 0.95; batch check time fell from 4 h to 25 min with outgoing Ra held at 0.12 nm.

Company
A semiconductor substrate maker, E. China
Address
Shanghai
MARSURF-UD130 for Nanometre Roughness of SiC Substrates
0.3 nmVertical resolution
0.12 nmOutgoing Ra

Polished 6-inch SiC substrates require Ra ≤0.2 nm. All checks were outsourced to AFM with a 4-hour turnaround per batch, so slurry recipe corrections lagged badly and outgoing Ra drifted between 0.10 and 0.18 nm.

Solution: a MARSURF-UD130 ultra-precision profilometer with 0.3 nm vertical resolution and a 0.05 mN measuring force to avoid scratching, grading Ra and Rq per ISO 4287. Five points per wafer (centre and edge), scanned at 0.1 mm/s to suppress vibration noise.

Results: same-wafer correlation with AFM reached 0.95 with deviation ≤0.02 nm. Batch turnaround fell to 25 minutes, slurry corrections moved three hours earlier, outgoing Ra stabilized at 0.12 nm, and epitaxy customer complaints dropped to zero.