Connectors2025

Lot monitoring of BeCu contact-spring microhardness

HVS-1000Z digital micro-Vickers tests 0.15 mm BeCu springs at HV0.2 on a vacuum thin-foil holder; after ageing they measured 380 HV0.2 with a 10-point lot spread within 15 HV.

Firma
A connector manufacturer, E. China
Adresse
Yueqing, Zhejiang
Lot monitoring of BeCu contact-spring microhardness
380 HV0.2Hardness after ageing
1 周 → 当天Turnaround

The 0.15 mm beryllium-copper contact springs in high-speed connectors get their contact force from ageing hardness. Outsourced testing took a week, and uneven clamping of the thin strip made readings jump around.

Solution: an HVS-1000Z digital micro-Vickers hardness tester at HV0.2 (1.961 N) with 10 s dwell, using a vacuum thin-foil holder to keep the strip level. Indentation spacing of at least 2.5 diagonals per GB/T 4340.1 is placed automatically.

Result: 380 HV0.2 after ageing with a 10-point lot spread within 15 HV; hardness correlated with measured spring force at r = 0.93, so rapid hardness checks now replace part of the full force testing.

Benefit: turnaround fell from a week to same-day, and lot-consistency complaints on springs dropped 70%.