Giám sát vi độ cứng lò xo đồng berili

HVS-1000Z đo lò xo BeCu 0,15 mm ở HV0.2, đạt 380 HV.

Công ty
Nhà máy đầu nối, Đông Trung Quốc
Địa chỉ
Nhạc Thanh, Chiết Giang
Giám sát vi độ cứng lò xo đồng berili
380 HV0.2Độ cứng sau tôi
1 周 → 当天Thời gian kiểm tra

The 0.15 mm beryllium-copper contact springs in high-speed connectors get their contact force from ageing hardness. Outsourced testing took a week, and uneven clamping of the thin strip made readings jump around.

Solution: an HVS-1000Z digital micro-Vickers hardness tester at HV0.2 (1.961 N) with 10 s dwell, using a vacuum thin-foil holder to keep the strip level. Indentation spacing of at least 2.5 diagonals per GB/T 4340.1 is placed automatically.

Result: 380 HV0.2 after ageing with a 10-point lot spread within 15 HV; hardness correlated with measured spring force at r = 0.93, so rapid hardness checks now replace part of the full force testing.

Benefit: turnaround fell from a week to same-day, and lot-consistency complaints on springs dropped 70%.