HOTY9025D Roundness Measuring Instrument
Roundness Measuring Instrument
- 主轴精度径向误差 / ±(0.025+5H/10000)μm
- 轴向误差±(0.025+6X/10000)μm
MARSURF-LD260 · 2026-11-17 · +86 21 5748 2007
Surface Roughness Tester
By submitting you agree to our privacy policy.
MARSURF LD 130 综合性轮廓和表面测量站
Mahr 度量先进的技术实现一步完成轮廓和粗糙度测量。MarSurf LD 130 和 LD 260 测量站经过系统化的设计以利用第一代设备的经验。
一步完成粗糙度和轮廓测量
高测量和定位速度可大幅减少测量时间
删除创新的测头系统
快速可靠的测杆更换,磁性支架同步检测测杆
长测量长度,高达 260 mm (MarSurf LD 260),测量行程 13 mm(100 mm 测杆长度)或 26 mm(200 mm 测杆长度)
模块结构,方便维护
维护时无需拆卸测量立柱
MARSURF-LD130/260 表面粗糙度轮廓仪技术参数:
测量速度(文本)
0.02mm/s至10mm/s;
粗糙度测量时推荐 0.1mm/s至0.5mm/s
扫描长度末尾(X 方向)
130 mm
分辨率
0.8 nm
扫描长度开始(X 方向)
0.1 mm
定位速度(文本)
0.02 mm/s 至 200 mm/s
测量范围 mm
13 mm (100 mm probe arm)
26 mm (200 mm probe arm)
扫描长度(文本)
0.1mm-130 mm 或260mm
测量力(N)
0.5 mN至30 mN,可软件调整
MARSURF-LD260 Surface Roughness Tester supplied by CHWES. 7 key specifications available on request.
| 扫描长度末尾(X 方向) | 130 mm |
|---|---|
| 分辨率 | 0.8 nm |
| 扫描长度开始(X 方向) | 0.1 mm |
| 定位速度(文本) | 0.02 mm/s 至 200 mm/s |
| 测量范围 mm | 13 mm (100 mm probe arm) 26 mm (200 mm probe arm) |
| 扫描长度(文本) | 0.1mm-130 mm 或260mm |
| 测量力(N) | 0.5 mN至30 mN,可软件调整 |
* Generated by rule engine over the product database; for pre-selection only.
A stylus instrument drags a diamond tip (2 or 5 µm radius) across the surface under constant force. The tip follows micro-relief, an inductive transducer converts displacement into a signal, and after amplification and filtering the profile is obtained. Per GB/T 10610 a Gaussian filter (or phase-corrected 2RC) with cut-off λc separates roughness from waviness; Ra, Rz, Rq, Rt and RSm are then computed over the sampling length.
Profile instruments share the same precision guide to capture roughness and macro profile, evaluating straightness, arc radius, angle, groove depth and pitch. Long-travel models (160–300 mm X, ±5 mm Z) suit shafts, rolls and mould surfaces.
1. Ra: arithmetic mean deviation, Ra = (1/n)Σ|zi| for sampled points; samples of 2, 4, 3, 5, 1 µm give Ra = 3 µm.
2. Rz: mean of the five highest peaks and five deepest valleys per sampling length (maximum peak-to-valley under GB/T 3505).
3. Rmr: material ratio curve at height c, describing the bearing capability of mating faces.
4. Filtering: Gaussian λc = 0.8/2.5/8 mm separates roughness from waviness; λs suppresses noise.
5. Roundness: least-squares centre, minimum-zone, minimum circumscribed or maximum inscribed; spindle error should be under 1/5 of the tolerance.
| Standard | Title | Use |
|---|---|---|
| GB/T 1031-2009 | Surface roughness — parameters and values | Parameter limits |
| GB/T 3505-2009 | Surface texture — profile terms | Terminology |
| GB/T 10610-2009 | Rules and procedures for assessment | Filtering, evaluation |
| ISO 4287 | Profile method — terms | Export projects |
| ISO 4288 | Rules and procedures | Sampling length |
1. Separate three quantities: roughness (Ra/Rz/Rmr, micrometre-scale microtexture), waviness (W, 0.1–10 µm mid-spatial), and form error (roundness, cylindricity, macro geometry). They need different instruments or filters.
2. Profilometers and roundness testers are not interchangeable: profilometers measure Ra/Rz and profile along a line (XZ, CX series); roundness testers measure roundness, cylindricity and coaxiality of bodies of revolution (Y90 series). A cylinder bore needing both requires two machines or a combined type.
3. Sensor range sets capability: ±50 µm suffices for Ra alone; deep grooves, steps and large arcs need ±500 µm or more; mirror surfaces below Ra 0.01 µm need low-noise sensors and isolation.
4. Travel and load: XZ-150 for small parts, XZ-230/XZ-150G for mid-size bores and shafts, Y901200 or custom stages above one metre.
5. Software must support the standards: full Ra/Rz/Rq/Rsk/Rku/Rmr per GB/T 1031 and ISO 4287; roundness per GB/T 7234 with minimum-zone, least-squares, minimum-circumscribed and maximum-inscribed evaluation.
6. On-site use: workshops need vibration and dust control; portable units (DY-300) suit large parts at lower accuracy.
| Model | Type | Capability | Typical parts |
|---|---|---|---|
| XZ-150 / XZ-150G | Roughness and profile | Ra/Rz + profile | Small precision parts |
| XZ-230 | Roughness and profile | Ra/Rz + long travel | Shafts, cylinder bores |
| CX-1(S) / CX-1(G) | Roughness | Ra/Rz/Rmr | Shop-floor sampling |
| CX-3/100 / CX-3/160 | Roughness and profile | Ra + profile + steps | Spools, sealing faces |
| 2207 / 2302A | Roundness | Roundness/cylindricity | Bearing rings, journals |
| Y9025B/C/D | Roundness | Roundness/coaxiality/waviness | Precision spindles, bores |
| Y9060 / Y901200 | Large roundness | Large-diameter roundness | Wind bearings, flanges |
| DY-300 | Portable | Ra/Rz | Large parts on site |
Why results disagree: wrong cut-off wavelength, insufficient evaluation length, mismatched stylus radius and an unlevelled part account for most disputes.
Preparation. Clean with ethanol to remove oil and chips; let the part stabilise to ambient (±2 °C); inspect the stylus at 20× for wear.
Settings. Choose λc to GB/T 1031 from expected Ra: 0.25 mm up to 0.1 µm, 0.8 mm for 0.1–2 µm, 2.5 mm for 2–10 µm, 8 mm above 10 µm; evaluation length 5 × λc.
Measurement. Stylus perpendicular to the lay, lower slowly, start when force is stable. Measure at least three positions per surface and average; on cylinders follow the generatrix.
Judgement. Compare with the drawing limit; no single reading should exceed 1.2 × the limit. Arbitrate with a profile instrument and a certified specimen.
Quality control. Daily check against Ra 0.4/1.6/6.3 specimens, recalibrate beyond 5% deviation, replace or verify the stylus every 12 months.