The plant had to verify the hot hardness of steam-generator tubes batch by batch through third-party labs, with a 21-day queue that threatened delivery milestones.
Solution: HMAS-HT900CM with an inert-gas circuit performs 10 kgf indents per ASTM E92 at 800℃, 6 points on each of 3 tube samples per batch, 15 s dwell, in-situ diagonal reading, and automatic HV10 reporting.
Result: batch mean at 800℃ was 152 HV10 with dispersion ≤3.5%, all above the specification floor. Testing cycle was cut by 90% and outsourcing cost was reduced by about RMB 600,000 per year.