Атомная энергетика2023

Твердость труб из сплава 690TT при 800℃

HMAS-HT900CM: контроль твердости труб 690TT при 800℃ по ASTM E92, цикл сокращён с 21 до 2 дней.

Компания
Производитель ядерного оборудования, Вост. Китай
Адрес
Шанхай
Твердость труб из сплава 690TT при 800℃
21 d → 2 dЦикл испытаний

The plant had to verify the hot hardness of steam-generator tubes batch by batch through third-party labs, with a 21-day queue that threatened delivery milestones.

Solution: HMAS-HT900CM with an inert-gas circuit performs 10 kgf indents per ASTM E92 at 800℃, 6 points on each of 3 tube samples per batch, 15 s dwell, in-situ diagonal reading, and automatic HV10 reporting.

Result: batch mean at 800℃ was 152 HV10 with dispersion ≤3.5%, all above the specification floor. Testing cycle was cut by 90% and outsourcing cost was reduced by about RMB 600,000 per year.