Năng lượng hạt nhân2023

Độ cứng ống hợp kim 690TT ở 800℃

HMAS-HT900CM kiểm tra độ cứng ống 690TT ở 800℃ theo ASTM E92, rút chu kỳ từ 21 xuống 2 ngày.

Công ty
Nhà máy thiết bị hạt nhân, Đông Trung Quốc
Địa chỉ
Thượng Hải
Độ cứng ống hợp kim 690TT ở 800℃
21 d → 2 dChu kỳ kiểm tra

The plant had to verify the hot hardness of steam-generator tubes batch by batch through third-party labs, with a 21-day queue that threatened delivery milestones.

Solution: HMAS-HT900CM with an inert-gas circuit performs 10 kgf indents per ASTM E92 at 800℃, 6 points on each of 3 tube samples per batch, 15 s dwell, in-situ diagonal reading, and automatic HV10 reporting.

Result: batch mean at 800℃ was 152 HV10 with dispersion ≤3.5%, all above the specification floor. Testing cycle was cut by 90% and outsourcing cost was reduced by about RMB 600,000 per year.