Nuclear energy2023

800℃ hot hardness verification of Alloy 690TT tubes

HMAS-HT900CM enabled in-house 800℃ hardness sampling of 690TT tubes per ASTM E92, cutting cycle time from 21 days to 2.

Company
A nuclear equipment manufacturer, E. China
Address
Shanghai
800℃ hot hardness verification of Alloy 690TT tubes
21 d → 2 dTesting cycle

The plant had to verify the hot hardness of steam-generator tubes batch by batch through third-party labs, with a 21-day queue that threatened delivery milestones.

Solution: HMAS-HT900CM with an inert-gas circuit performs 10 kgf indents per ASTM E92 at 800℃, 6 points on each of 3 tube samples per batch, 15 s dwell, in-situ diagonal reading, and automatic HV10 reporting.

Result: batch mean at 800℃ was 152 HV10 with dispersion ≤3.5%, all above the specification floor. Testing cycle was cut by 90% and outsourcing cost was reduced by about RMB 600,000 per year.