Nodularity was judged by outsourced metallography with a 2-day delay, so failed heats had already been poured into castings, costing over one million RMB per year.
Solution: the MMAS-4 inverted metallurgical microscope with a furnace-side rapid polishing stand rates graphite morphology per GB/T 9441 at 100X on unetched samples, with 500X verification of pearlite; 2 samples per heat, 5 fields each.
Result: judgment time fell from 2 days to 15 minutes, with 98% agreement against third-party labs for grade 3 and above. Scrap from poor nodularization fell from 1.8% to 0.3% in the same year.