Литейное производство2023

Оценка шаровидного графита в чугуне

MMAS-4: оценка чугуна QT450-10 по GB/T 9441 за 15 мин у печи.

Компания
Литейный завод автозапчастей, Вост. Китай
Адрес
Аньхой
Категория
Микроскопы
Оценка шаровидного графита в чугуне
2 d → 15 minВремя оценки
1.8% → 0.3%Уровень брака

Nodularity was judged by outsourced metallography with a 2-day delay, so failed heats had already been poured into castings, costing over one million RMB per year.

Solution: the MMAS-4 inverted metallurgical microscope with a furnace-side rapid polishing stand rates graphite morphology per GB/T 9441 at 100X on unetched samples, with 500X verification of pearlite; 2 samples per heat, 5 fields each.

Result: judgment time fell from 2 days to 15 minutes, with 98% agreement against third-party labs for grade 3 and above. Scrap from poor nodularization fell from 1.8% to 0.3% in the same year.

⇄0СравнениеСравнение характеристик