Đúc và luyện kim2023

Đánh giá độ cầu hóa gang cầu

MMAS-4 đánh giá QT450-10 theo GB/T 9441 trong 15 phút tại lò.

Công ty
Nhà máy đúc phụ tùng ô tô, Đông Trung Quốc
Địa chỉ
An Huy
Danh mục
Kính hiển vi
Đánh giá độ cầu hóa gang cầu
2 d → 15 minThời gian đánh giá
1.8% → 0.3%Tỷ lệ phế phẩm

Nodularity was judged by outsourced metallography with a 2-day delay, so failed heats had already been poured into castings, costing over one million RMB per year.

Solution: the MMAS-4 inverted metallurgical microscope with a furnace-side rapid polishing stand rates graphite morphology per GB/T 9441 at 100X on unetched samples, with 500X verification of pearlite; 2 samples per heat, 5 fields each.

Result: judgment time fell from 2 days to 15 minutes, with 98% agreement against third-party labs for grade 3 and above. Scrap from poor nodularization fell from 1.8% to 0.3% in the same year.

⇄0So sánhSo sánh thông số