6013 and 5052 aluminium sheets for phone mid-frames were co-stored and visually identical. Once, 5052 was machined as 6013 and the whole anodized batch showed colour mismatch - a single loss over 800000 yuan.
Solution: a Q2 portable OES stationed at receiving, with an argon cylinder cart, quantifies Si, Mg, Cu, Mn and Fe with a 3-second spark. The built-in grade library identifies 1xxx-7xxx aluminium alloys and gives a conformance verdict.
Results: 100% non-destructive screening replaced sample-and-send testing. Three mixed-material batches were intercepted in the first year, including 6063 passed off as 6061, avoiding about 2.6 million yuan of direct loss; incoming inspection fell from two days to two hours.