3C electronics2023

Q2 OES for Alloy Grade ID of 3C Housings

Q2 portable OES identifies 5xxx/6xxx aluminium grades in 3 s at receiving, quantifying Si, Mg and Cu; non-destructive checks intercepted 3 mixed-material batches, avoiding about 2.6 million yuan of loss.

Company
A 3C precision structure maker, S. China
Address
Dongguan, Guangdong
Q2 OES for Alloy Grade ID of 3C Housings
3 sID time per spot
3 批Mixed batches caught

6013 and 5052 aluminium sheets for phone mid-frames were co-stored and visually identical. Once, 5052 was machined as 6013 and the whole anodized batch showed colour mismatch - a single loss over 800000 yuan.

Solution: a Q2 portable OES stationed at receiving, with an argon cylinder cart, quantifies Si, Mg, Cu, Mn and Fe with a 3-second spark. The built-in grade library identifies 1xxx-7xxx aluminium alloys and gives a conformance verdict.

Results: 100% non-destructive screening replaced sample-and-send testing. Three mixed-material batches were intercepted in the first year, including 6063 passed off as 6061, avoiding about 2.6 million yuan of direct loss; incoming inspection fell from two days to two hours.

⇄0CompareProduct comparison