Điện tử 3C2023

Quang phổ Q2 nhận diện mác hợp kim vỏ 3C

Quang phổ Q2 cầm tay nhận diện hợp kim 5xxx/6xxx trong 3 s; chặn 3 lô trộn liệu, tránh thiệt hại 2,6 triệu tệ.

Công ty
Nhà máy kết cấu 3C, Nam Trung Quốc
Địa chỉ
Đông Quan, Quảng Đông
Quang phổ Q2 nhận diện mác hợp kim vỏ 3C
3 sThời gian nhận diện
3 批Lô trộn đã chặn

6013 and 5052 aluminium sheets for phone mid-frames were co-stored and visually identical. Once, 5052 was machined as 6013 and the whole anodized batch showed colour mismatch - a single loss over 800000 yuan.

Solution: a Q2 portable OES stationed at receiving, with an argon cylinder cart, quantifies Si, Mg, Cu, Mn and Fe with a 3-second spark. The built-in grade library identifies 1xxx-7xxx aluminium alloys and gives a conformance verdict.

Results: 100% non-destructive screening replaced sample-and-send testing. Three mixed-material batches were intercepted in the first year, including 6063 passed off as 6061, avoiding about 2.6 million yuan of direct loss; incoming inspection fell from two days to two hours.

⇄0So sánhSo sánh thông số