Автокомпоненты2024

Кругломер Y9025C для коренных шеек коленвала

Кругломер Y9025C с точностью шпинделя 0,02 мкм выявил вибрацию шлифования 0,4 мкм, Cpk круглости вырос до 1,67.

Компания
Завод коленчатых валов, Вост. Китай
Адрес
Сучжоу, Цзянсу
Кругломер Y9025C для коренных шеек коленвала
0.02 μmТочность шпинделя
1.67Cpk круглости

The plant graded main-journal roundness per GB/T 1182 by outsourcing 24-point CMM fits. Readings scattered, high-frequency lobing was invisible, and dynamometer tests had shown abnormal journal wear.

Solution: a Y9025C roundness tester with an air-bearing spindle of 0.02 um rotational accuracy. After centering and levelling, roundness, cylindricity and waviness were evaluated per GB/T 7235 with a 500 UPR filter; three sections per journal, 3600 points per revolution, a full crankshaft in 15 minutes.

Results: journal roundness was corrected from the fitted 2.1 um to a true 0.9 um, and a 15 UPR grinding chatter component of 0.4 um was identified. After setting the wheel dressing depth to 2 um, batch roundness Cpk rose from 1.12 to 1.67 and abnormal wear on the dynamometer disappeared.

⇄0СравнениеСравнение характеристик