Phụ tùng ô tô2024

Máy đo độ tròn Y9025C cho cổ trục khuỷu

Y9025C độ chính xác trục 0,02 um phát hiện vân rung mài 0,4 um, Cpk độ tròn đạt 1,67.

Công ty
Nhà máy trục khuỷu, Đông Trung Quốc
Địa chỉ
Tô Châu, Giang Tô
Máy đo độ tròn Y9025C cho cổ trục khuỷu
0.02 μmĐộ chính xác trục chính
1.67Cpk độ tròn

The plant graded main-journal roundness per GB/T 1182 by outsourcing 24-point CMM fits. Readings scattered, high-frequency lobing was invisible, and dynamometer tests had shown abnormal journal wear.

Solution: a Y9025C roundness tester with an air-bearing spindle of 0.02 um rotational accuracy. After centering and levelling, roundness, cylindricity and waviness were evaluated per GB/T 7235 with a 500 UPR filter; three sections per journal, 3600 points per revolution, a full crankshaft in 15 minutes.

Results: journal roundness was corrected from the fitted 2.1 um to a true 0.9 um, and a 15 UPR grinding chatter component of 0.4 um was identified. After setting the wheel dressing depth to 2 um, batch roundness Cpk rose from 1.12 to 1.67 and abnormal wear on the dynamometer disappeared.

⇄0So sánhSo sánh thông số