Precision sectioning plus vacuum mounting delivers results in 35 minutes with hole-copper repeatability within 1.5 µm, replacing a three-day outsourced cycle.

Компания
PCB manufacturer, Jiangsu
Адрес
Suzhou, Jiangsu
PCB micro-sectioning for hole-wall copper and resin voids
3 d → 35 minPer board
≤1.5 μmCopper repeatability
约 45 万元Annual saving

Multilayer boards require hole-wall copper of at least 20 µm with resin voids and delamination judged to IPC-TM-650. Outsourcing took three days and CNY 800 per board, far too slow when the process drifted.

Solution: an in-house metallography room with HXQ-50 precision sectioning through the hole centre at 200 rpm, vacuum mounting to keep resin out of the barrel, grinding to the centreline and a 5 s micro-etch, then measurement of wall copper, inner-layer copper and voids on HX-G3A.

Result: 35 minutes per board with repeatability within 1.5 µm; one batch at 16 µm was traced to low plating current density and corrected within four hours, avoiding about 2000 m² of scrap, and outsourcing cost fell by roughly CNY 450k a year.