Cutting tools2024

Microhardness and bonding quality of TiAlN tool coatings

HMAS-D1000SMZ automatic microhardness tester measures TiAlN coatings at HV0.05 with auto-focus indentation reading; the coating measured 3180-3260 HV0.05 without substrate breakthrough.

회사명
A precision cutting-tool plant, S. China
주소
Dongguan, Guangdong
카테고리
Hardness Testers
Microhardness and bonding quality of TiAlN tool coatings
3180~3260 HV0.05Coating hardness
-60%Chipping complaints

The milling cutters carry a 3 µm TiAlN coating that must verify at 3000 HV or more. The previous HV0.3 load made diagonals longer than half the coating thickness, so substrate influence dragged readings low and scattered them.

Solution: an HMAS-D1000SMZ fully automatic micro-Vickers tester with a minimum force of 0.098 N; HV0.05 with 10 s dwell was chosen here. Auto-focus and automatic indentation recognition are used, and the load was checked against the GB/T 4340.1 rule that indentation depth stay below one tenth of coating thickness.

Result: the coating measured 3180-3260 HV0.05 with an 80 HV spread over five points; deviation from the coating supplier data stayed within 3%.

Benefit: incoming coating inspection is now evidence-based, and early chipping complaints from soft coatings fell 60%.