Dụng cụ cắt2024

Đo vi độ cứng lớp phủ TiAlN trên dao

HMAS-D1000SMZ đo TiAlN ở HV0.05, đạt 3180-3260 HV.

Công ty
Nhà máy dao chính xác, Nam Trung Quốc
Địa chỉ
Đông Quan, Quảng Đông
Đo vi độ cứng lớp phủ TiAlN trên dao
3180~3260 HV0.05Độ cứng lớp phủ
-60%Khiếu nại mẻ

The milling cutters carry a 3 µm TiAlN coating that must verify at 3000 HV or more. The previous HV0.3 load made diagonals longer than half the coating thickness, so substrate influence dragged readings low and scattered them.

Solution: an HMAS-D1000SMZ fully automatic micro-Vickers tester with a minimum force of 0.098 N; HV0.05 with 10 s dwell was chosen here. Auto-focus and automatic indentation recognition are used, and the load was checked against the GB/T 4340.1 rule that indentation depth stay below one tenth of coating thickness.

Result: the coating measured 3180-3260 HV0.05 with an 80 HV spread over five points; deviation from the coating supplier data stayed within 3%.

Benefit: incoming coating inspection is now evidence-based, and early chipping complaints from soft coatings fell 60%.