Cutting tools2025

HXSQ-100F Precision Sectioning of Tool Coatings

HXSQ-100F low-speed sectioning avoids chipping on TiAlN-coated inserts; optical measurement on mounted cross-sections reads 3.0±0.3 um, replacing indirect XRF conversion and raising batch conformance from 88% to 99%.

회사명
A coated cutting tool maker, E. China
주소
Changzhou, Jiangsu
HXSQ-100F Precision Sectioning of Tool Coatings
3.0±0.3 μmCoating thickness
99%Batch conformance

TiAlN coating thickness was measured by XRF, whose conversion factors for curved cutting edges drifted with substrate composition - up to 15% off true section values - causing both chipping from over-thick coatings and early wear from thin ones.

Solution: an HXSQ-100F precision cutter with a low-speed diamond blade and automatic feed sections coated inserts without edge chipping or delamination. After hot mounting and polishing to 1 um, coating thickness and interface integrity are read directly at 500X.

Results: measured thickness holds 3.0±0.3 um; grade-specific correction factors from section data brought XRF agreement within 3%. Batch thickness conformance rose from 88% to 99% and chipping complaints dropped 55% quarter on quarter.