HXSQ-100F cắt dao phủ TiAlN không mẻ; dày 3,0±0,3 um trên mặt cắt, tỷ lệ đạt từ 88% lên 99%.

Công ty
Nhà máy phủ dao, Đông Trung Quốc
Địa chỉ
Thường Châu, Giang Tô
HXSQ-100F cắt mặt cắt lớp phủ dao
3.0±0.3 μmĐộ dày lớp phủ
99%Tỷ lệ đạt

TiAlN coating thickness was measured by XRF, whose conversion factors for curved cutting edges drifted with substrate composition - up to 15% off true section values - causing both chipping from over-thick coatings and early wear from thin ones.

Solution: an HXSQ-100F precision cutter with a low-speed diamond blade and automatic feed sections coated inserts without edge chipping or delamination. After hot mounting and polishing to 1 um, coating thickness and interface integrity are read directly at 500X.

Results: measured thickness holds 3.0±0.3 um; grade-specific correction factors from section data brought XRF agreement within 3%. Batch thickness conformance rose from 88% to 99% and chipping complaints dropped 55% quarter on quarter.