Cemented carbide2023

Incoming HV30 re-verification of cemented-carbide inserts

HVS-30Z digital Vickers re-verifies carbide inserts at HV30 to GB/T 4340.1, 294.2 N load with 15 s dwell, agreeing with supplier certificates within 20 HV and rejecting two overstated lots.

회사명
A cemented-carbide tool company, S. China
주소
Zhuzhou, Hunan
카테고리
Hardness Testers
Incoming HV30 re-verification of cemented-carbide inserts
≤20 HVCertificate deviation
2Rejected lots

The company used to release carbide inserts on supplier certificates alone, until a batch chipping incident showed actual hardness far below the certificate. An HV30 re-verification capability was urgent, yet the brittle alloy chips at indentation edges, making readings hard.

Solution: an HVS-30Z digital Vickers hardness tester at HV30 (294.2 N) with 15 s dwell and a 0.1 µm measuring eyepiece. Per GB/T 4340.1 the specimen thickness must be at least 1.5 diagonals; chipped indentations are voided and re-made, and three points per insert are averaged.

Result: YG8 inserts measured 1520-1560 HV30, within 20 HV of supplier certificates; two consecutive lots reading only 1380 HV were rejected as overstated.

Benefit: incoming re-verification intercepted the overstated inserts, and batch chipping incidents have not recurred.

⇄0비교사양 비교