Hợp kim cứng2023

Kiểm tra lại HV30 mảnh dao hợp kim cứng

HVS-30Z kiểm tra HV30 theo GB/T 4340.1, lệch ≤20 HV.

Công ty
Công ty dao hợp kim cứng, Nam Trung Quốc
Địa chỉ
Chu Châu, Hồ Nam
Kiểm tra lại HV30 mảnh dao hợp kim cứng
≤20 HVLệch chứng nhận
2Lô bị từ chối

The company used to release carbide inserts on supplier certificates alone, until a batch chipping incident showed actual hardness far below the certificate. An HV30 re-verification capability was urgent, yet the brittle alloy chips at indentation edges, making readings hard.

Solution: an HVS-30Z digital Vickers hardness tester at HV30 (294.2 N) with 15 s dwell and a 0.1 µm measuring eyepiece. Per GB/T 4340.1 the specimen thickness must be at least 1.5 diagonals; chipped indentations are voided and re-made, and three points per insert are averaged.

Result: YG8 inserts measured 1520-1560 HV30, within 20 HV of supplier certificates; two consecutive lots reading only 1380 HV were rejected as overstated.

Benefit: incoming re-verification intercepted the overstated inserts, and batch chipping incidents have not recurred.