HOTHMAS-D5/10/30/50SZA Vickers Hardness Tester
Vickers Hardness Tester
- 测量分析系统HMAS‑硬度测量分析系统
- 光学成像系统维氏硬度大三通光学成像系统
ZHR-150SS · 2026-11-17 · +86 21 5748 2007
Rockwell Hardness Tester
By submitting you agree to our privacy policy.
电脑全洛氏硬度计为研润自主研发第五代高端产品,采用笔记本电脑控制,操作简单方便。实现了自动打压、自动计算硬度值。操作简单方便。操作面板采用菜单式结构,具有良好的可靠性,可操作性和直观性。
适用于金属材料的洛氏硬度试验。本系列洛氏硬度计操作简便迅速,性能稳定,使用广泛。可进行黑色金属和有色金属的洛氏硬度测定,广泛适用于工厂车间和计量部门.
性能特点:
1、笔记本电脑控制;
2、闭环传感器控制系统,无需砝码;
3、无需特殊安装,甚至无需售后;
4、无需施加初始试验力,自动加卸试验力;
5、测量精度高,硬度值自动修正;
6、测试过程中显示实时曲线;
7、随时将数据导入电脑;
8、硬度标尺选择时,提示选用压头;
硬度计的技术参数:
1、洛氏总试验力:表面洛氏15Kg(147.1N),30Kg(294.2N),45Kg(441.3N)
洛氏 60kgf (588.4N)、100kgf (980.7N)、150kgf (1471N)
2、硬度测量范围:洛氏HRA:20~88 、HRB:20~100、HRC:20~70
表面洛氏HR15N:70~91、HR30N:42~80、HR45N:20~70)
表面洛氏HR15T:73~93、HR30T:43~82、HR45T:12~72)
3、执行国家标准GB/T230.2国家标准,JJG112检定规程
4、洛氏标尺:洛氏15种HRA、HRB、HRC、HRD、HRE、HRF、HRG、HRH、HRK、HRL、HRM、HRP、HRR、HRS、HRV
表面洛氏15种;HR15N、HR30N、HR45N、HR15T、HR30T、HR45T、
HR15W、HR30W、HR45W、HR15X、HR30X、HR45X、HR15Y、HR30Y、HR45Y
5、被测试件允许最大高度:220mm
6、压头中心到机身距离:200mm
7、硬度计外形尺寸(长×宽×高)560×250×800(mm)
8、电源电压:AC220V±5%,50~60Hz
9、延时控制:1~60秒可调
标准配置:
1、主机 1台
2、电脑(硬度测量系统软件(已装到电脑) 1台
3、金刚石洛氏压头 1只
4、直径1.5875mm球压头 1只
5、大平试台、中平试台、“V”型试台 共3只
6、标准洛氏硬度块 6块
7、保险丝 2根
8、电源线 1根
9、U盘 1只
10、底脚螺钉 4只
11、防尘袋 1只
12、产品合格证书 1份
13、产品使用说明书 1本
ZHR-150SS Rockwell Hardness Tester supplied by CHWES. 15 key specifications available on request.
| 洛氏总试验力 | 表面洛氏15Kg(147.1N),30Kg(294.2N),45Kg(441.3N);洛氏 60kgf (588.4N)、100kgf (980.7N)、150kgf (1471N) |
|---|---|
| 硬度测量范围 | 洛氏HRA:20~ |
| HRB | 20~1 |
| HRC | 20~70 |
| 表面洛氏HR15N | 70~ |
| HR30N | 42~ |
| HR45N | 20~70) |
| 表面洛氏HR15T | 73~ |
| HR30T | 43~ |
| HR45T | 12~72);执行国家标准GB/T230.2国家标准,JJG112检定规程 |
| 洛氏标尺 | 洛氏15种HRA、HRB、HRC、HRD、HRE、HRF、HRG、HRH、HRK、HRL、HRM、HRP、HRR、HRS、HRV;表面洛氏15种;HR15N、HR30N、HR45N、HR15T、HR30T、HR45T |
| 被测试件允许最大高度 | 220mm |
| 压头中心到机身距离 | 200mm;硬度计外形尺寸(长×宽×高)560×250×800(mm) |
| 电源电压 | AC220V±5%,50~60Hz |
| 延时控制 | 1~60秒可调 |
* Generated by rule engine over the product database; for pre-selection only.
Hardness testing presses an indenter into the surface under a constant load and converts indentation size or depth into a hardness value. Vickers uses a 136° diamond pyramid: HV = 0.1891 × F(N)/d²(mm), where d is the mean diagonal.
Hot hardness is performed in vacuum or high-purity inert gas. Specimen and indenter are heated independently and must be at the same temperature or corrected per the standard; loading, dwell and unloading all happen inside the hot zone, and the indentation is measured through a high-temperature optic or after cooling. The HMAS series uses a uniform hot zone with ±5 °C uniformity from 200 to 1600 °C.
1. Rockwell: HR = K − h/0.002 (K = 100 for HRC, 130 for HRB). At h = 0.078 mm, HRC = 61.
2. Brinell: HBW = 2F/(πD(D−√(D²−d²))); with F=1838.6 N, D=2.5 mm, d=1.1 mm, HBW ≈ 192.
3. Vickers: HV = 0.1891·F/d² (F in N); F=9.807 N with d=0.05 mm gives HV ≈ 742.
4. Test forces: choose Brinell loads by 0.045F/D²; Rockwell 10 kgf preliminary with 60/100/150 kgf total; surface scales 3 / 15/30/45 kgf.
5. Conversions: HRC ≈ HBW/10 only as a rough mid-range guide — official reports must follow the GB/T 1172 tables.
| Standard | Title | Scope |
|---|---|---|
| GB/T 4340.1-2009 | Vickers hardness test — test method | Vickers |
| GB/T 230.1-2018 | Rockwell hardness test | Rockwell |
| GB/T 231.1-2018 | Brinell hardness test | Brinell |
| ISO 6507-1 | Vickers hardness test | Export |
| ASTM E92 | Vickers hardness of metallic materials | Americas |
| GB/T 17394.1-2014 | Leeb hardness test | Portable |
Hot hardness has no unified national standard; ASTM E92 practice is normally cited with temperature, atmosphere, dwell and indenter material stated in the report.
1. Principle follows the target: Rockwell for macro hardness and heat-treatment acceptance; Brinell for cast iron, annealed and forged parts where a large indent is representative; Vickers or micro-Vickers for thin layers, coatings and small areas.
2. Bench or portable: bench units (HRC-150SMJ, HBRVS-187.5) where parts can be brought in; portable Leeb for large moulds, in-service piping and non-removable parts, corrected against a bench reference, typically within ±2 HRC.
3. One for many: mixed, low-volume shops do well with a Brinell-Vickers-Rockwell combination unit covering HRA/HRB/HRC/HV/HB.
4. Automation: manual below 100 parts per operator per day; motorised elevation, automatic loading and data upload (HRC-150SMJ) above 200 or for unattended runs.
5. Reference blocks: two to three blocks covering the working range, checked every shift and sent for annual calibration.
6. Specimen requirements: Rockwell needs thickness at least ten times the indent depth and Ra ≤1.6 µm; otherwise switch to Vickers or superficial Rockwell.
| Model | Principle | Range | Typical use |
|---|---|---|---|
| HRC-150SMJ | Rockwell, motorised digital | HRA/HRB/HRC | Batch sampling in heat treatment |
| HRC-150SM / HRC-150M | Rockwell | HRA/HRB/HRC | Incoming and in-process checks |
| HRC-45M | Superficial Rockwell | 15N/30N/45N | Sheet, plating, case layers |
| HRS-150M / XHRS-150M | Digital Rockwell | HRA/HRB/HRC | Lines needing data upload |
| HBRVS-187.5 | Brinell-Vickers-Rockwell | HBW/HRA/HRB/HRC/HV | Mixed low-volume production |
Three rules for trustworthy data: check the reference block every shift and record it; keep the support face flat and clean; keep indent spacing at least three indent diameters.
Specimen. Test and support faces parallel; thickness at least 1.5 × diagonal (Vickers) or 10 × depth (Rockwell); Ra ≤ 0.4 µm, free of scale and oil.
Room temperature. Select load, apply within 10–15 s, dwell 10–15 s, unload, measure diagonals. Spacing between indentations ≥3d, from the edge ≥2.5d.
Hot hardness. Load the specimen, evacuate or backfill argon, ramp and soak 20–30 min, lower the indenter, load and dwell, unload, cool or measure hot, then apply the temperature correction.
Gradient. Step every 0.05–0.1 mm to the hardness plateau; determine effective case depth at 550 HV1 per GB/T 9450.
Quality control. Check a certified block (e.g. 700 HV1) each shift, recalibrate beyond ±3%, and log furnace curves and atmosphere for hot tests.