HB-2 Brinell Hardness Tester

Brinell Hardness Tester

ModellHB-2
  • 测量范围450HBS以下
  • 钢球直径Φ10毫米
  • 外形尺寸Φ30X120毫米
  • 读数显微镜尺寸155X85毫米

By submitting you agree to our privacy policy.

01

Überblick

HB-2锤击式布氏硬度计是以一定直径的钢球在施以瞬间的冲击载荷后,使钢球压入工件,获取相应的数据,再通过压痕测量,获取相应的数据,再通过查表即可获得试件的硬度值.本硬度计构造简单,便于携带,使用方便,是工矿企业、生产车间、材料车间、材料仓库等测量布氏硬度理想的硬度计.
性能特点:
HB-2锤击式布氏硬度计适用范围:
1.在天然状态或退火状态下钢的布氏硬度值与抗拉强度值(限于非奥氏体钢)
2.在精练淬火或淬火加回火状态下钢的布氏硬度值与抗拉强度值(限与非奥氏体钢)
3.铸铁的布氏硬度值
4.黄铜铸件的布氏硬度值
5.辗压黄铜的布氏硬度值
6.紫铜的布氏硬度值
7.锡青铜合金的布氏硬度值
8.铝合金铸件的布氏硬度值
HB-2锤击式布氏硬度计主要技术规格:
1、测量范围:450HBS以下
2、钢球直径:Φ10毫米
3、外形尺寸:Φ30X120毫米
4、读数显微镜尺寸:155X85毫米
5、重量:约0.6千克

HB-2 Brinell Hardness Tester supplied by CHWES. 5 key specifications available on request.

02

Technische Daten

测量范围450HBS以下
钢球直径Φ10毫米
外形尺寸Φ30X120毫米
读数显微镜尺寸155X85毫米
重量约0.6千克

* Generated by rule engine over the product database; for pre-selection only.

03

Messprinzip

Hardness testing presses an indenter into the surface under a constant load and converts indentation size or depth into a hardness value. Vickers uses a 136° diamond pyramid: HV = 0.1891 × F(N)/d²(mm), where d is the mean diagonal.

Hot hardness is performed in vacuum or high-purity inert gas. Specimen and indenter are heated independently and must be at the same temperature or corrected per the standard; loading, dwell and unloading all happen inside the hot zone, and the indentation is measured through a high-temperature optic or after cooling. The HMAS series uses a uniform hot zone with ±5 °C uniformity from 200 to 1600 °C.

  • Vickers 0.01–100 kgf: full range, thin layers and case-depth gradients.
  • Rockwell C 150 kgf: fast batch checking of hardened parts.
  • Brinell: castings, annealed and coarse-grain materials.
  • Leeb: portable rebound testing on large parts.
04

Process animation

  1. Preparation: polish to Ra ≤ 0.4 µm, remove work-hardened layers.
  2. Mount and align: place the specimen, position the indenter over the test point.
  3. Heat up (hot hardness): evacuate to ≤10⁻² Pa or backfill argon, ramp and soak.
  4. Load: apply force at the set rate, dwell 10–15 s.
  5. Measure: read diagonals or depth, compute HV/HRC.
  6. Gradient: step along depth and plot hardness versus distance.
0102030405
05

Calculation & formulas

1. Rockwell: HR = K − h/0.002 (K = 100 for HRC, 130 for HRB). At h = 0.078 mm, HRC = 61.

2. Brinell: HBW = 2F/(πD(D−√(D²−d²))); with F=1838.6 N, D=2.5 mm, d=1.1 mm, HBW ≈ 192.

3. Vickers: HV = 0.1891·F/d² (F in N); F=9.807 N with d=0.05 mm gives HV ≈ 742.

4. Test forces: choose Brinell loads by 0.045F/D²; Rockwell 10 kgf preliminary with 60/100/150 kgf total; surface scales 3 / 15/30/45 kgf.

5. Conversions: HRC ≈ HBW/10 only as a rough mid-range guide — official reports must follow the GB/T 1172 tables.

06

Normen

StandardTitleScope
GB/T 4340.1-2009Vickers hardness test — test methodVickers
GB/T 230.1-2018Rockwell hardness testRockwell
GB/T 231.1-2018Brinell hardness testBrinell
ISO 6507-1Vickers hardness testExport
ASTM E92Vickers hardness of metallic materialsAmericas
GB/T 17394.1-2014Leeb hardness testPortable

Hot hardness has no unified national standard; ASTM E92 practice is normally cited with temperature, atmosphere, dwell and indenter material stated in the report.

07

Auswahl

1. Principle follows the target: Rockwell for macro hardness and heat-treatment acceptance; Brinell for cast iron, annealed and forged parts where a large indent is representative; Vickers or micro-Vickers for thin layers, coatings and small areas.

2. Bench or portable: bench units (HRC-150SMJ, HBRVS-187.5) where parts can be brought in; portable Leeb for large moulds, in-service piping and non-removable parts, corrected against a bench reference, typically within ±2 HRC.

3. One for many: mixed, low-volume shops do well with a Brinell-Vickers-Rockwell combination unit covering HRA/HRB/HRC/HV/HB.

4. Automation: manual below 100 parts per operator per day; motorised elevation, automatic loading and data upload (HRC-150SMJ) above 200 or for unattended runs.

5. Reference blocks: two to three blocks covering the working range, checked every shift and sent for annual calibration.

6. Specimen requirements: Rockwell needs thickness at least ten times the indent depth and Ra ≤1.6 µm; otherwise switch to Vickers or superficial Rockwell.

ModelPrincipleRangeTypical use
HRC-150SMJRockwell, motorised digitalHRA/HRB/HRCBatch sampling in heat treatment
HRC-150SM / HRC-150MRockwellHRA/HRB/HRCIncoming and in-process checks
HRC-45MSuperficial Rockwell15N/30N/45NSheet, plating, case layers
HRS-150M / XHRS-150MDigital RockwellHRA/HRB/HRCLines needing data upload
HBRVS-187.5Brinell-Vickers-RockwellHBW/HRA/HRB/HRC/HVMixed low-volume production

Three rules for trustworthy data: check the reference block every shift and record it; keep the support face flat and clean; keep indent spacing at least three indent diameters.

08

Prüfverfahren

Specimen. Test and support faces parallel; thickness at least 1.5 × diagonal (Vickers) or 10 × depth (Rockwell); Ra ≤ 0.4 µm, free of scale and oil.

Room temperature. Select load, apply within 10–15 s, dwell 10–15 s, unload, measure diagonals. Spacing between indentations ≥3d, from the edge ≥2.5d.

Hot hardness. Load the specimen, evacuate or backfill argon, ramp and soak 20–30 min, lower the indenter, load and dwell, unload, cool or measure hot, then apply the temperature correction.

Gradient. Step every 0.05–0.1 mm to the hardness plateau; determine effective case depth at 550 HV1 per GB/T 9450.

Quality control. Check a certified block (e.g. 700 HV1) each shift, recalibrate beyond ±3%, and log furnace curves and atmosphere for hot tests.

09

Industry applications

  • Heat-treatment shops: Rockwell HRC sampling of quenched and tempered parts, carburised surface hardness, Brinell HBW on annealed stock.
  • Castings and forgings: body hardness and HAZ values, section hardness gradients indicating cooling rate and structural uniformity.
  • Moulds and tools: HRC versus wear resistance after hardening and tempering, edge-to-core hardness difference on cutting tools.
  • Thin and small parts: case-hardened layers, coatings and sheet need Vickers or superficial Rockwell (HBRVS-187.5 covers HRA/HRB/HRC/HV/HB).
  • Bearings and gears: ring and raceway hardness, case-to-core difference against carburising requirements.
  • Pressure vessels and piping: weld and HAZ hardness to detect brittle microstructures, typically ≤350 HV10.
  • Incoming verification: hardness as the fastest screening method when material grades are mixed, confirmed by OES.
  • Field and in-service: portable Leeb or ultrasonic hardness testers on large immovable parts, corrected against a bench reference.
10

Price and lead time for this model

By submitting you agree to our privacy policy.

⇄0VergleichTechnischer Vergleich