During coating validation for customers, the provider lacked a unified wear measurement basis; different inspectors chose different tool-change moments, scattering life data.
Solution: the BID-300 measuring microscope with crosshair eyepiece and digital micrometer reads VB at the middle of the flank wear land per ISO 3685, sampling every 15 cutting minutes, with VB=0.3 mm as the unified failure criterion.
Result: wear curves of three coating formulations became comparable for the first time; the best formulation raised tool life from 95 to 128 minutes (+35%), and the report was used directly for customer acceptance.