Cutting tool manufacturing2023

On-line flank wear VB tracking of milling inserts

BID-300 tracks flank wear per ISO 3685 with VB=0.3 mm criterion; after coating optimization, tool life rose 35%.

会社名
A tool coating service provider, SW China
所在地
Chongqing
カテゴリ
Microscopes
On-line flank wear VB tracking of milling inserts
+35%Tool life gain

During coating validation for customers, the provider lacked a unified wear measurement basis; different inspectors chose different tool-change moments, scattering life data.

Solution: the BID-300 measuring microscope with crosshair eyepiece and digital micrometer reads VB at the middle of the flank wear land per ISO 3685, sampling every 15 cutting minutes, with VB=0.3 mm as the unified failure criterion.

Result: wear curves of three coating formulations became comparable for the first time; the best formulation raised tool life from 95 to 128 minutes (+35%), and the report was used directly for customer acceptance.

⇄0比較仕様比較