Sản xuất dụng cụ cắt2023

Theo dõi mòn VB mảnh phay

BID-300 theo dõi mòn VB theo ISO 3685, tuổi dao tăng 35%.

Công ty
Đơn vị phủ dụng cụ, Tây Nam Trung Quốc
Địa chỉ
Trùng Khánh
Danh mục
Kính hiển vi
Theo dõi mòn VB mảnh phay
+35%Tăng tuổi dao

During coating validation for customers, the provider lacked a unified wear measurement basis; different inspectors chose different tool-change moments, scattering life data.

Solution: the BID-300 measuring microscope with crosshair eyepiece and digital micrometer reads VB at the middle of the flank wear land per ISO 3685, sampling every 15 cutting minutes, with VB=0.3 mm as the unified failure criterion.

Result: wear curves of three coating formulations became comparable for the first time; the best formulation raised tool life from 95 to 128 minutes (+35%), and the report was used directly for customer acceptance.

⇄0So sánhSo sánh thông số