Connector terminals are 0.15 mm thick; worn cutting edges cause burrs and width drift. The plant used to stop the line and check with calipers, and escapes still reached the customer.
Solution: a YRVMS3020CNC beside the press with a fixed eight-dimension program. Five parts every two hours feed SPC; CPK below 1.33 raises an alarm; burr height is measured with coaxial light against a 0.03 mm limit.
Result: customer PPM fell from 1200 to 180, die regrinding moved from a fixed 300,000 strokes to CPK-triggered maintenance, and die life improved by 18%.