Precision stamping2024

In-line sampling and die-wear trending for high-speed stamping

Five parts every two hours with a live CPK dashboard moved die maintenance from calendar-based to condition-based.

회사명
Connector stamping plant, Jiangsu
주소
Kunshan, Jiangsu
In-line sampling and die-wear trending for high-speed stamping
180Customer PPM
+18%Die life

Connector terminals are 0.15 mm thick; worn cutting edges cause burrs and width drift. The plant used to stop the line and check with calipers, and escapes still reached the customer.

Solution: a YRVMS3020CNC beside the press with a fixed eight-dimension program. Five parts every two hours feed SPC; CPK below 1.33 raises an alarm; burr height is measured with coaxial light against a 0.03 mm limit.

Result: customer PPM fell from 1200 to 180, die regrinding moved from a fixed 300,000 strokes to CPK-triggered maintenance, and die life improved by 18%.

⇄0비교사양 비교