Construction rebar2024

One-way tensile testing of rebar taper-thread splices

WAW-600D tests rebar taper-thread splices one-way to JGJ 107, 600 kN covering 40 mm splices, automatically judging whether fracture is in the bar or the splice, with reports to the site platform.

Firma
A construction engineering test centre, E. China
Adresse
Nanjing, Jiangsu
One-way tensile testing of rebar taper-thread splices
600 kNCapacity
6 minTime per specimen

Site taper-thread couplers are sampled one set of three per 500 splices for one-way tensile tests to JGJ 107. The centre previously logged fracture position by hand, so disputed lots lacked curve evidence and reports carried little weight.

Solution: a WAW-600D servo-hydraulic universal testing machine, 600 kN class 0.5 with load indication error within ±0.5%. The software embeds JGJ 107 logic, records the full force-displacement curve, and automatically flags fracture in the parent bar, the thread runout or coupler slip, then assigns the splice grade.

Result: a 32 mm HRB400E splice measured 612 MPa tensile strength, fractured in the parent bar and graded Class I; six minutes per specimen, with curves and reports archived straight to the site testing platform.

Benefit: disputed lots can be reviewed from stored curves; annual testing disputes dropped to zero and report acceptance improved markedly.