Строительная арматура2024

Растяжение резьбовых соединений арматуры

WAW-600D 600 кН: растяжение соединений по JGJ 107 до Ø40 мм.

Компания
Строительная испытательная лаборатория, Вост. Китай
Адрес
Нанкин, Цзянсу
Растяжение резьбовых соединений арматуры
600 kNДиапазон
6 minВремя на образец

Site taper-thread couplers are sampled one set of three per 500 splices for one-way tensile tests to JGJ 107. The centre previously logged fracture position by hand, so disputed lots lacked curve evidence and reports carried little weight.

Solution: a WAW-600D servo-hydraulic universal testing machine, 600 kN class 0.5 with load indication error within ±0.5%. The software embeds JGJ 107 logic, records the full force-displacement curve, and automatically flags fracture in the parent bar, the thread runout or coupler slip, then assigns the splice grade.

Result: a 32 mm HRB400E splice measured 612 MPa tensile strength, fractured in the parent bar and graded Class I; six minutes per specimen, with curves and reports archived straight to the site testing platform.

Benefit: disputed lots can be reviewed from stored curves; annual testing disputes dropped to zero and report acceptance improved markedly.