Thép cốt bê tông2024

Thử kéo mối nối ren thép cốt bê tông

WAW-600D 600 kN thử mối nối theo JGJ 107 đến φ40.

Công ty
Trung tâm kiểm định xây dựng, Đông Trung Quốc
Địa chỉ
Nam Kinh, Giang Tô
Thử kéo mối nối ren thép cốt bê tông
600 kNDải đo
6 minThời gian/mẫu

Site taper-thread couplers are sampled one set of three per 500 splices for one-way tensile tests to JGJ 107. The centre previously logged fracture position by hand, so disputed lots lacked curve evidence and reports carried little weight.

Solution: a WAW-600D servo-hydraulic universal testing machine, 600 kN class 0.5 with load indication error within ±0.5%. The software embeds JGJ 107 logic, records the full force-displacement curve, and automatically flags fracture in the parent bar, the thread runout or coupler slip, then assigns the splice grade.

Result: a 32 mm HRB400E splice measured 612 MPa tensile strength, fractured in the parent bar and graded Class I; six minutes per specimen, with curves and reports archived straight to the site testing platform.

Benefit: disputed lots can be reviewed from stored curves; annual testing disputes dropped to zero and report acceptance improved markedly.

⇄0So sánhSo sánh thông số