Foundry2025

90-second melt analysis cuts trimming laps

A TY-9620 at the furnace returns 18 elements in 90 s before tapping, cutting trim adjustments by 65%.

Firma
Automotive foundry, East China
Adresse
Changshu, Jiangsu
90-second melt analysis cuts trimming laps
90 sMelt analysis time
0.2%Out-of-spec rejects

Sending samples to the central lab took 15 minutes round trip while the furnace idled hot.

Solution: a floor-standing TY-9620 on the melt platform with plumbed argon, two-point type standardisation each shift; sample → ground face → 18-element result in 90 s.

Result: trimming laps down 65%, out-of-spec rejects from 0.8% to 0.2%, and about ¥96 k/month saved in alloy and power.