A DN2400 flange arrived with suspected distortion of the gasket face; returning it would have cost three weeks.
Solution: the MC003-SCANARM scanned the whole face at 1 mm spacing on site and measured bevel angles and root faces, producing a colour map in 30 minutes.
Result: flatness 0.08 mm against a 0.10 mm limit and bevels within 30°±1° — no rework, schedule saved, roughly ¥1.2 M avoided.