Energy & heavy equipment2024

Portable-arm measurement of site flanges and pipe bevels

The MC003-SCANARM verified flatness of a DN2400 flange gasket face and bevel angles on site, avoiding a ¥1.2 M rework.

회사명
Chemical-plant contractor, coastal China
주소
Ningbo, Zhejiang
Portable-arm measurement of site flanges and pipe bevels
0.08 mmFace flatness
¥1.2 MRework avoided

A DN2400 flange arrived with suspected distortion of the gasket face; returning it would have cost three weeks.

Solution: the MC003-SCANARM scanned the whole face at 1 mm spacing on site and measured bevel angles and root faces, producing a colour map in 30 minutes.

Result: flatness 0.08 mm against a 0.10 mm limit and bevels within 30°±1° — no rework, schedule saved, roughly ¥1.2 M avoided.