Hộp số ô tô2025

MARSURF-XC2 đo nhám mặt răng bánh răng

MARSURF-XC2 đầu dò nhỏ đo Ra/Rz/RSm theo ISO 4288; Ra 0,19 um, khiếu nại tiếng rít giảm 70%.

Công ty
Nhà máy bánh răng hộp số, Nam Trung Quốc
Địa chỉ
Quảng Châu, Quảng Đông
MARSURF-XC2 đo nhám mặt răng bánh răng
0.19 μmRa mặt răng
0.33%Tỷ lệ khiếu nại rít

After grinding, flank roughness was spot-checked with a portable tester whose stylus could not enter tooth spaces below module 2, so measurements were taken on tip lands instead. True flank condition was out of control and gearbox whine complaints ran at 1.1%.

Solution: a MARSURF-XC2 roughness station with a small-bore stylus and a tooth-locating fixture, tracing along the flank line and grading Ra, Rz and RSm per ISO 4288 with 0.8 mm sampling and 4 mm evaluation lengths; three gears per batch, four flanks each.

Results: the true flank Ra of 0.19 um (versus 0.35 um proxy readings) is now held stable with RSm within 0.06 mm. The wheel dressing interval was optimized from 8 h to 6.5 h, whine complaints fell to 0.33%, and annual warranty cost dropped by about 1.2 million yuan.

⇄0So sánhSo sánh thông số