Stainless steel fabrication2024

HXZMP-1000 for Stainless Weld Metallography

HXZMP-1000 with 10% oxalic electrolytic etch prepares 304 stainless weld samples showing weld, HAZ and base metal in one clear field; ferrite reads 6.2% by point count, doubling prep efficiency.

회사명
A stainless pressure fittings maker, E. China
주소
Taizhou, Jiangsu
HXZMP-1000 for Stainless Weld Metallography
6.2%Ferrite content
40 件Samples per day

304 stainless welded pipe needs metallographic checks of weld structure and ferrite content before shipping. The grinder and polisher sat in separate rooms, samples shuttled between them, and scratches at the fusion line were misread by a customer as lack-of-fusion defects.

Solution: an HXZMP-1000 combined grinder-polisher runs 240, 600 and 1200 grit papers then 3 um and 1 um diamond; electrolytic etching in 10% oxalic acid at 6 V for 15 s reveals weld dendrites, HAZ and base metal in one field.

Results: fusion-line boundaries are clean and artefact-free; ferrite measures 6.2% by point counting, inside the 3-10% process window. Prep throughput doubled to 40 weld samples a day, and annual customer quality disputes fell from six to one.

⇄0비교사양 비교