Gia công thép không gỉ2024

HXZMP-1000 chuẩn bị mẫu mối hàn inox

HXZMP-1000 ăn mòn điện giải oxalic mẫu hàn 304; ferrit 6,2% theo đếm điểm, hiệu suất gấp đôi.

Công ty
Nhà máy phụ kiện inox, Đông Trung Quốc
Địa chỉ
Thái Châu, Giang Tô
HXZMP-1000 chuẩn bị mẫu mối hàn inox
6.2%Hàm lượng ferrit
40 件Mẫu mỗi ngày

304 stainless welded pipe needs metallographic checks of weld structure and ferrite content before shipping. The grinder and polisher sat in separate rooms, samples shuttled between them, and scratches at the fusion line were misread by a customer as lack-of-fusion defects.

Solution: an HXZMP-1000 combined grinder-polisher runs 240, 600 and 1200 grit papers then 3 um and 1 um diamond; electrolytic etching in 10% oxalic acid at 6 V for 15 s reveals weld dendrites, HAZ and base metal in one field.

Results: fusion-line boundaries are clean and artefact-free; ferrite measures 6.2% by point counting, inside the 3-10% process window. Prep throughput doubled to 40 weld samples a day, and annual customer quality disputes fell from six to one.

⇄0So sánhSo sánh thông số