Metrology2023

Building a Brinell hardness verification facility in a metrology lab

HBS-3000MV digital Brinell tester with reference blocks and a standard measuring device performs HBW 10/3000 dissemination to JJG 150, indication error within ±1%, passing the standard-establishment assessment first time.

회사명
A metrology and test station, E. China
주소
Zhenjiang, Jiangsu
카테고리
Hardness Testers
Building a Brinell hardness verification facility in a metrology lab
≤±1%Indication error
约 200 台Annual verifications

The station needed a public Brinell hardness standard covering HBW 10/3000 and HBW 2.5/187.5. The old tester repeated poorly, and annual drift of the reference blocks could not be monitored.

Solution: an HBS-3000MV digital Brinell hardness tester with nine force steps from 62.5 to 3000 kgf, dwell settable from 1 to 60 s, and automatic indentation-diameter measurement. Second-class reference blocks support periodic checks, and verification to JJG 150 covers indication error and repeatability.

Result: at HBW 10/3000 the indication error is within ±1% with repeatability within 1.5% and dwell-time error of ±0.5 s; the standard-establishment assessment passed first time.

Benefit: local enterprises can now have Brinell testers verified on site, about 200 instruments per year.