Đo lường2023

Xây dựng thiết bị kiểm định máy Brinell

HBS-3000MV truyền chuẩn HBW 10/3000 theo JJG 150, sai số ≤±1%.

Công ty
Trạm đo lường, Đông Trung Quốc
Địa chỉ
Trấn Giang, Giang Tô
Xây dựng thiết bị kiểm định máy Brinell
≤±1%Sai số chỉ thị
约 200 台Kiểm định mỗi năm

The station needed a public Brinell hardness standard covering HBW 10/3000 and HBW 2.5/187.5. The old tester repeated poorly, and annual drift of the reference blocks could not be monitored.

Solution: an HBS-3000MV digital Brinell hardness tester with nine force steps from 62.5 to 3000 kgf, dwell settable from 1 to 60 s, and automatic indentation-diameter measurement. Second-class reference blocks support periodic checks, and verification to JJG 150 covers indication error and repeatability.

Result: at HBW 10/3000 the indication error is within ±1% with repeatability within 1.5% and dwell-time error of ±0.5 s; the standard-establishment assessment passed first time.

Benefit: local enterprises can now have Brinell testers verified on site, about 200 instruments per year.