Hydraulics2025

Combined Ra and Rmr evaluation solves an out-of-spec leakage problem

CX-3/100 showed Ra within spec but Rmr only 42%, indicating an insufficient plateau; after honing adjustment leakage fell 60%.

회사명
Hydraulic valve maker, Jiangsu
주소
Wuxi, Jiangsu
Combined Ra and Rmr evaluation solves an out-of-spec leakage problem
42% → 68%Rmr(2cr)
-60%Leakage
72% → 96%Bench pass

Spool OD roughness had to be Ra 0.2–0.4 µm and every reading was inside that band, yet bench leakage stayed high, suggesting many peaks and little bearing area.

Solution: CX-3/100 measuring Rmr, Rpk and Rvk alongside Ra/Rz to ISO 13565 for plateau assessment, plus profile roundness and straightness.

Result: Ra 0.31 µm passed but Rmr(2cr) was only 42% against a 60% requirement, a classic unremoved-peak condition; after changing honing stone grit and stroke speed Rmr reached 68%, leakage dropped 60% and bench first-pass rate rose from 72% to 96%.