Automotive2023

Fast sampling of key dimensions on seatbelt retractor stampings

YR3020Z zoom vision measures hole pitch, flange height and bend angle on retractor brackets in 50 seconds, repeatability within 3 µm, replacing calipers plus a projector.

会社名
An automotive safety-parts plant, E. China
所在地
Wuxi, Jiangsu
Fast sampling of key dimensions on seatbelt retractor stampings
6 min → 50 sTime per piece
0.03 → 0.005 mmOperator difference

The seatbelt retractor bracket is a 2.5 mm high-strength steel stamping with a hole-pitch tolerance of ±0.06 mm. Calipers plus a projector took six minutes per piece, and the two inspectors often disagreed, causing disputes on borderline parts.

Solution: a YR3020Z manual zoom vision machine with a 6.5:1 continuous zoom lens, transmitted plus ring illumination, measuring hole pitch, flange height and bend angle in one clamping; X/Y indication error is ±(3+L/200) µm, and the software judges against the tolerance band automatically.

Result: 50 seconds per piece with repeatability within 3 µm; the inspector-to-inspector difference fell from 0.03 mm to below 0.005 mm.

Benefit: sampling frequency tightened from every two hours to every 30 minutes, so early die wear is caught half a shift sooner.

⇄0比較仕様比較