Fasteners2025

Bolt metallographic preparation from 25 minutes per piece to six pieces in eight minutes

HXZDQ-160 mounting with HXZMP-3000 automatic polishing completes six samples in 40 minutes with decarburisation repeatability within 0.01 mm.

会社名
Fastener testing centre, Hebei
所在地
Handan, Hebei
Bolt metallographic preparation from 25 minutes per piece to six pieces in eight minutes
30 → 110 件Throughput
25 → 6.7 minPer sample
≤0.01 mmRepeatability

The centre handles 40–60 bolts a day for decarburisation, carburisation and laps. Single-platen manual polishing took 25 minutes per piece, two inspectors managed 30 a day, and uneven hand pressure skewed decarburisation readings.

Solution: HXQ-50 precision sectioning to avoid overheating, HXZDQ-160 mounting six at a time, HXZMP-3000 automatic polishing with four grinding and two diamond steps under programmed force and time, then 4% nital etch.

Result: six samples in 40 minutes, about 6.7 minutes each, raising daily throughput from 30 to 110; decarburisation repeatability within 0.01 mm; one inspector now handles preparation while the other moves to data analysis.