Metallurgy / rolls2025

Combined Ra and crown profile measurement on ground rolls

The CX-3/160 measures Ra and crown in one setup, cutting inspection from 35 to 12 minutes.

会社名
Cold roll maker, Jiangsu
所在地
Wuxi, Jiangsu
Combined Ra and crown profile measurement on ground rolls
12 minInspection time
2.1%Rework rate

Cold rolls require Ra 0.2–0.4 µm and 0.05 mm crown. The plant used a portable roughness tester plus分段 micrometer readings: two setups, 35 minutes, and no way to detect grinding chatter.

Solution: a CX-3/160 profile instrument with 160 mm travel, one setup scanning along the generatrix, outputting Ra/Rz and the crown curve together; the software overlays the theoretical crown and flags deviation above 0.01 mm.

Result: 12 minutes per roll, chatter detected reliably, and the grinding rework rate fell from 6% to 2.1%.