Four Roundness Evaluation Methods: Minimum Zone versus Least Squares
One section, four reference circles, four roundness values; minimum zone…
Test method · Working principle

One section, four reference circles, four roundness values; minimum zone…

One cutoff step off shifts Ra by 30 %: the cutoff decides which undulati…

Ra is the arithmetic mean, Rz the ten-point height, Rt the total peak-to…

UCI senses the resonance shift of a rod under a Vickers diamond to infer…

Nitrided case depth uses core hardness +50 HV or 550 HV as threshold; th…

Below a 20 μm diagonal the measurement error climbs steeply; choose the …

Leeb is a dynamic rebound method needing specimens of 2 kg and 5 mm mini…

Thickness first, then case depth: thick coarse parts take Brinell, routi…

Class 1 machines require ±1.0 % force error and 1.0 % repeatability, ver…

The S-N curve splits into low- and high-cycle regimes; R=σmin/σmax gover…

Rp0.2 needs a class 0.5 extensometer with gauge-length error within ±1 %…

Method A closes the loop on extensometer strain, giving the tightest sca…